Mining Plant Horizontal Vacuum Belt Filter Press
Filter press cloth is mainly applied to filter press, including chamber filter press, membrane filter press, recessed, plate and frame, etc.
Belt filter cloth is mainly applied to horizontal belt filter, belt filter press, monobelt filter. The 95 series filter belt and double layer monofilament filter cloth is our patent products. Manufactured with special raw materials and weaving technics, the cloths have good resistence to both acid and alkali. The dimensional stability is perfect because of the special style of the strenghth, tightness, thickness and etc.
Monofilament & Multifilament filter cloth: have good air and water permeability.They have good ability to prevent the granules from blocking in the fabrics and the filter cakes can be peeled off easily, therefore, they can be used time after time.
P006MD-P140D double layer monofilament filter cloth are mainly applied to belt filters, other products can be applied to plate and frame, recessed and membrane filter presses.
Chemical:
Catalyst, cobalt carbonate, zinc oxide, zirconium carbonate, activated carbon, cobalt carbonate, borate, dyes and intermediates, iron oxide, nickle, salt, aluminum oxide, titanium dioxide, additives, glycerol, pesticides, white carbon black, zinc, calcium carbonate, etc.
Mining:
Red mud, tailings gold, potash fertilizer, vanadium ore, the end of coal, clean coal, clay, Kaolin clay, etc.
Metallurgical:
Gold, molybdenum, lead, vanadium, nickel, zinc, copper, tungsten, carbide slag, etc.
Food
Fruite juice, suger, starch, sweetener, beer, etc.
Environmental protection:
Sewage treatment, slude dewatering, flue gas desulphurization, salt mud, fly ash, etc.
Property |
Polyester (PE) |
Polypropylene |
Nylon |
Acid |
Excellent |
Excellent |
Excellent |
Alkali |
Average |
Excellent |
Excellent |
Electrical Conductivity |
Poor |
Good |
Average |
Elongation |
30%-40% |
Better than PE |
Poor |
Recovery |
Excellent |
Slightly better than PE |
Poor |
Abrasion |
Excellent |
Good |
Excellent |
Heat Resistance |
150 °C |
90 °C |
100 °C |
Softening point |
230 -240 °C |
140 -150 °C |
200 °C |
Melting point |
255 -265 °C |
165 -170 °C |
220 °C |